Surface treatment is a process technology that changes the surface morphology, organizational structure, or chemical composition of materials through physical, chemical, or mechanical methods, thereby endowing components with specific surface properties. In the field of mechanical manufacturing, surface treatment is directly related to the wear resistance, corrosion resistance, fatigue resistance, surface hardness, and decorative effect of components. This article systematically analyzes typical process methods in the surface treatment industry and their performance requirements for components, focusing on the specific applications of various components in core process links such as shot blasting cleaning and strengthening, coating and pretreatment, electroplating and chemical plating, anodizing, thermal spraying, chemical heat treatment (carburizing, nitriding, carbonitriding), and surface inspection. The article elaborates on the technical characteristics and selection principles of surface treatment components from the perspectives of component material selection, process equipment configuration, quality inspection and control. Combined with the development trends of environmental protection, energy conservation, and intelligence, it looks forward to the technological evolution direction of surface treatment components, providing reference for surface treatment process optimization and equipment selection.


14.jpg


1. Introduction

Surface treatment is an indispensable link in the mechanical manufacturing chain. The vast majority of components often fail on the surface during use - corrosion begins on the surface, wear occurs on the contact surface, and fatigue cracks often originate on the surface. Therefore, improving the surface performance of components through surface treatment is an economically effective means to extend product life and enhance reliability. At the same time, surface treatment also plays a role in improving appearance, cleaning and removing dirt, and providing a foundation for subsequent coating.

According to different mechanisms of action, surface treatment processes can be roughly divided into the following categories: surface cleaning and roughening (shot blasting, sandblasting, polishing, acid washing), surface coating preparation (electroplating, chemical plating, thermal spraying, anodizing, micro arc oxidation, vapor deposition), surface modification (chemical heat treatment such as carburizing, nitriding, laser surface treatment, ion implantation), and surface coating (spraying, immersion coating, electrophoresis, electrostatic powder spraying). The performance requirements for tooling equipment components vary greatly among different processes, but the commonality is that the performance of key components in the process equipment (such as shot blasting blades, spray gun nozzles, electroplating anodes, heat treatment fixtures, coating conveyor chains, etc.) directly determines the quality, efficiency, and cost of surface treatment.

In recent years, with increasingly strict environmental regulations and higher requirements for surface quality in the manufacturing industry, the surface treatment industry is undergoing a profound transformation from traditional high pollution processes to green, intelligent, and precise directions. This transformation places higher demands on the materials, structure, lifespan, and automation level of surface treated components. This article will focus on the main process areas of surface treatment and systematically analyze the application practices and technological developments of various components.

2、 Components in surface cleaning and roughening processes

Surface cleaning is the process of removing oxide scale, rust, old coatings, oil stains, and burrs from the surface of a workpiece, while also providing the required surface roughness for subsequent painting or plating. Shot blasting and sandblasting are the main mechanical cleaning methods.

2.1 Core components in shot blasting cleaning equipment

The shot blasting machine uses a high-speed rotating shot blasting wheel to eject steel shot or steel wire cutting shot at a speed of 50-110m/s onto the surface of the workpiece, achieving cleaning and strengthening. The key components of a shot blasting machine include blades, dividing wheels, directional sleeves, and impeller bodies.

The blade is the most severely worn component in the shot blasting machine. Early blades were made of high chromium cast iron (Cr15-Cr28, HRC58-62), with a lifespan of approximately 200-500 hours. Modern high-efficiency shot blasting equipment uses tungsten carbide hard alloy composite blades - covered with tungsten carbide welding layer or embedded with hard alloy blocks on the blade working surface, the blade life can be extended to 1500-3000 hours, greatly reducing the frequency of downtime and replacement. The shape design of the blades has evolved from straight blades to curved blades. Curved blades can accelerate projectiles more smoothly on the blades, reduce turbulence and energy loss, and improve ejection efficiency by about 15% to 20%.

The shot wheel controls the flow rate and velocity of the shot entering the blade, and its window size and shape affect the uniformity of the shot blasting flow. A gap of 0.2-0.5mm should be maintained between the inner hole of the pill wheel and the feeding tube. A gap that is too small can easily get stuck, while a gap that is too large can cause pill leakage. The pellet wheel is generally made of high chromium wear-resistant cast iron and needs to be replaced in a timely manner after wear, otherwise it will cause uneven ejection and a mottled cleaning effect on the surface of the workpiece.

The angle of the window of the directional sleeve determines the direction in which the projectile is ejected, and adjusting the position of the window of the directional sleeve can change the position of the projectile belt on the workpiece. The clearance between the directional sleeve and the dividing wheel is also controlled at 0.2-0.5mm. When cleaning complex shaped workpieces, it is necessary to use a dual shot blasting or multi shot blasting layout, with the directional sleeve angles of each shot blasting set separately to achieve comprehensive coverage of various parts of the workpiece.

The wear-resistant lining plate protects the shot blasting machine casing from being penetrated by the projectile. Manganese steel lining plate (ZGMn13) has good work hardening ability, and the surface hardness can be increased from HB200 to above HB500 after impact; Ceramic lining plates (alumina or silicon carbide) have better wear resistance but greater brittleness, making them suitable for areas with less impact; Rubber composite lining plate has both wear-resistant and shock-absorbing properties, which can reduce shot blasting noise and has gradually been promoted and applied.

2.2 Components in Sandblasting Equipment

Sandblasting uses compressed air as the driving force to rapidly spray abrasives (quartz sand, corundum, steel sand, glass beads, plastic particles, etc.) onto the surface of the workpiece. Its key components include nozzles, sand valves, sandblasting tanks, and protective equipment.

The sandblasting nozzle is the component with the fastest wear and tear. Traditional nozzles are made of boron carbide (B ₄ C), which is second only to diamond in hardness and has a lifespan of about 150-300 hours. However, it is brittle and not suitable for high-pressure sandblasting. Hard alloy nozzles (WC Co) have good toughness and a lifespan of 300-500 hours. Alumina ceramic nozzles are inexpensive, but have a lifespan of only 50-100 hours, making them suitable for intermittent operations. The nozzle inner hole shape is divided into Venturi type and straight hole type - Venturi nozzle increases the abrasive outlet velocity through a contraction expansion structure, and the cleaning efficiency can be improved by more than 30% under the same air pressure.

The sand valve adjusts the mixing ratio of abrasive and air. Excessive abrasive flow can clog pipelines, while insufficient flow can result in low efficiency. The ideal sand valve should be able to achieve stepless adjustment and the valve core should be wear-resistant. Ceramic core sand valves have become mainstream due to their good wear resistance and sensitive adjustment.

In the context of green environmental protection, wet sandblasting (spraying abrasive mixed with water with minimal dust) has been promoted. The internal structure of the nozzle needs to adapt to liquid-solid two-phase flow, and the material requirements are erosion resistance. Zirconia ceramics have become the preferred material for wet spray nozzles due to their good balance of toughness and wear resistance.

3、 Components in Painting and Pre treatment Processes

Coating is the main means of endowing components with anti-corrosion and decorative properties, and the quality of coating largely depends on the pre-treatment effect and the performance of spraying equipment.

3.1 Pre coating treatment equipment components

Pre coating treatment (degreasing, acid washing, phosphating or silanization) involves a series of tanks and conveying devices. Conveyor chains and hanging fixtures are key logistics components. For mass-produced automotive parts, a stacked suspension conveyor chain is used. The design of the chain pitch, load-bearing roller bearings, and hooks must consider the weight of the workpiece and the temperature of the tank solution (usually 50-55 ℃ for phosphating tanks). The contact point between the hanging fixture and the workpiece should be as small as possible to avoid the formation of blind spots in the coating process; For complex shaped workpieces, specialized elastic claws or magnetic suction cups need to be designed.

The tank heating tube is used to maintain the temperature of the process tank. Stainless steel heat exchange tubes (304 or 316L) may corrode in both acidic and alkaline solutions, while polytetrafluoroethylene (PTFE) coated heat exchange tubes or all PTFE heat exchangers may have slightly lower heat transfer efficiency but excellent corrosion resistance, making them standard configurations for high-end pre-treatment lines.

Spray pipes and nozzles are responsible for cleaning and surface adjustment functions in spray pre-treatment. The angle layout of the nozzle should ensure that all surfaces of the workpiece can be covered by the spray without blind spots. Nozzle blockage is a common malfunction, therefore the internal flow channel of the nozzle should be designed with an anti blockage structure (such as a tapered and expanding flow channel), and the mesh size of the pre filter should be selected according to the nozzle aperture (usually 1/3 to 1/2 of the nozzle aperture).

3.2 Spray equipment components

The core components of an air spray gun include a nozzle assembly (air cap, liquid nozzle, needle valve). The precise combination of the three determines the atomization effect and spray width shape. The nozzle aperture (0.8-2.5mm) is selected based on the viscosity and flow rate of the coating; The design of the main atomization holes, auxiliary atomization holes, and angle control holes distributed on the air cap affects the particle size and spray amplitude of the paint mist (circular, elliptical, or fan-shaped). The nozzle material is usually hardened stainless steel or hard alloy to resist the wear of hard pigments (such as titanium dioxide) in the coating.

The electrostatic spray gun adds an electrostatic generating device to the air spray gun. The gun body is equipped with a high-voltage electrostatic generator (output voltage of 30-100kV), which makes the atomized paint particles negatively charged, and the workpiece is grounded to form a positive electric field. The paint is electrostatically adsorbed onto the surface of the workpiece. The electrostatic confinement effect can significantly improve coating efficiency (from 40% to 60% in ordinary air spraying to 70% to 85%), reducing coating waste and environmental pollution. The key components of an electrostatic spray gun include high-voltage cables, electrode needles (usually tungsten needles, resistant to discharge erosion), and insulation materials (requiring a volume resistivity>10 ¹⁴Ω· cm and a withstand voltage>100kV).

Electrostatic powder spray gun is used for powder coating spraying. Its core is the high-voltage electrostatic generator and the powder charging structure inside the gun body (frictional charging or corona charging). The design of the nozzle (or electrode cover) of the powder spray gun needs to consider powder flow rate, charging efficiency, and spray amplitude control. The gun body material must be made of wear-resistant and anti stick engineering plastics (such as polytetrafluoroethylene composite nylon) to prevent powder adhesion and blockage.

The components of the paint supply system include paint pumps (diaphragm pumps or plunger pumps), pressure regulating valves, filters, and paint pipelines. The diaphragm material of the diaphragm pump needs to be resistant to solvent corrosion (such as Teflon or fluororubber), and the pump body material (aluminum alloy, stainless steel or polypropylene) should be selected according to the type of coating - water-based coatings have higher corrosion resistance requirements for pump body materials than solvent based coatings.

3.3 Curing equipment components

The coated workpiece needs to be baked to cure the coating. The key components of the curing oven include heating elements, circulating fans, and air duct systems.

Infrared heating elements (quartz lamps or ceramic infrared plates) are used for rapid heating, and their wavelength needs to match the absorption peak of the coating - water-based coatings have a high absorption rate for mid wave infrared (2-4 μ m), while solvent based coatings respond well to short wave infrared (0.8-2 μ m). The lifespan of infrared lamps is about 5000-8000 hours, and the pollutants deposited on the surface of the lamp will reduce radiation efficiency, requiring regular cleaning.

The high-temperature resistant fan (working temperature 150-250 ℃) and filter in the hot air circulation system are the core components to ensure uniform temperature and clean air inside the furnace. The fan bearings need to be equipped with high-temperature lubricating grease or independent water cooling, and filters (high-temperature fiberglass filter material) to prevent dust from contaminating the coating surface.

4、 Components in Electroplating and Chemical Plating Processes

Electroplating is a process of depositing metal coatings (zinc, copper, nickel, chromium, tin, etc.) on the surface of workpieces through electrolytic action, widely used to improve corrosion resistance, decorative properties, conductivity, and wear resistance.

4.1 Plating tank and anode components

The electroplating tank body is usually made of polypropylene (PP) or polyvinyl chloride (PVC) plastic plates welded together, and is equipped with heating tubes, anode conductive bars, cathode moving mechanisms, and filtration systems.

Soluble anode is a component in electroplating that dissolves and replenishes the coated metal. Taking chrome plating as an example, lead tin (containing 7% to 10% tin) or lead antimony (containing 6% to 8% antimony) alloy anodes have good conductivity and corrosion resistance, but lead anodes can produce lead pollution and are gradually replaced by titanium based ruthenium iridium oxide (DSA, size stable anode). DSA anodes are stable in size, insoluble, and pollution-free, but their price is relatively high. The shape and layout of the anode should be designed according to the geometric shape of the workpiece - complex workpieces require auxiliary anodes or pictographic anodes to ensure uniform current distribution and consistent coating thickness.

The cathode hanger is used to clamp workpieces and introduce current. The hanging material requires good conductivity, corrosion resistance, and no displacement reaction with the coated metal. Copper hangers with insulation layer (PVC or chloroprene rubber) are commonly used structures, and the exposed contact parts are made of phosphor bronze or stainless steel. The design of the hanger should consider current capacity, clamping reliability, and plating solution flow field - the contact resistance between the hanger hook and the cathode conductive rod should be less than 0.1m Ω, otherwise the contact point will heat up or even ignite, affecting the quality of the coating.

4.2 Filtering and Circulation System Components

Solid impurities in the plating solution, such as anode mud, dust, and burrs from falling workpieces, can cause roughness, pinholes, and pitting in the coating. The precision filter is the core equipment for removing these impurities, and its key components include the filter element (filtration accuracy of 1-10 μ m), pump body (corrosion-resistant magnetic pump), and filtration pipeline.

The filter element is selected based on the characteristics of the electroplating solution: cotton thread wound filter element is economical and suitable, but the filtration accuracy is relatively low (10-25 μ m); Polypropylene melt blown filter cartridge has an accuracy of 5-10 μ m and good chemical stability; The folding microporous filter cartridge has a filtration accuracy of 0.5-1 μ m and is suitable for processes such as bright nickel plating and chrome plating that require extremely high surface quality. The filter element needs to be cleaned or replaced regularly. When the pressure difference between the inlet and outlet reaches 0.15-0.2MPa, it indicates that the filter element is clogged.

The circulating pump must be selected as a leak free magnetic drive pump, and the pump body material is polypropylene or polyvinylidene fluoride (PVDF). The impeller, shaft sleeve, and thrust ring are all corrosion-resistant engineering plastics or silicon carbide. The isolation sleeve of the magnetic pump is a weak link, and once it breaks, it will cause leakage of the pump body. Therefore, high-strength ceramic or silicon carbide isolation sleeves are the choice for high reliability electroplating lines.

4.3 Power Supply and Electronic Control Components

The core components of electroplating power supply (rectifier) include rectifier transformer, rectifier diode (or thyristor), filter reactor, and cooling device.

High frequency switching power supplies are gradually replacing traditional thyristor power supplies due to their small size, high efficiency, and low ripple coefficient (<1%). The heat dissipation design of its internal power module (IGBT or MOSFET) is crucial - air-cooled models require smooth air ducts, while water-cooled models require deionized water circulation cooling. The connection between the output terminal and the anode and cathode must use copper bars or large section cables, and the connection should be silver plated or tin plated to reduce contact resistance. The ripple of electroplating power supply, especially low-frequency ripple, can cause coarse grains and increased stress in the coating. When used for precision electroplating, LC filtering devices need to be configured.

5、 Components in anodizing and microarc oxidation processes

The anodizing treatment of aluminum alloys is widely used in the fields of aerospace, 3C electronics, and automotive components, and its process equipment components have their own characteristics.

5.1 Anodizing tank and cathode components

The cathode plate is usually made of aluminum alloy sheet (6061 or 1060) or lead plate. Aluminum cathodes dissolve in sulfuric acid anodizing tanks, and it is necessary to regularly remove the oxide film generated on the stripped surface (which has high resistance and affects conductivity); Lead cathodes have good corrosion resistance, but they can cause lead pollution. Titanium cathode plate (pure titanium or titanium alloy) has excellent corrosion resistance and long service life due to the dense oxide film formed on the surface, and has become a standard configuration for high-end anodizing lines. The cathode plate area should be larger than the workpiece area, and the ratio of the two areas is usually between 1:1 and 2:1 to ensure uniform power lines.

Cooling system components are crucial. Anodizing is a strongly exothermic reaction (releasing approximately 0.54kcal of heat per ampere hour). If not cooled in time, the tank temperature will rapidly rise (the oxide film will become soft and the wear resistance will decrease when it exceeds 23 ℃, and the film layer will pulverize when it exceeds 30 ℃). Generally, titanium heat exchangers (serpentine coils or plate heat exchangers) are used in conjunction with refrigeration units to control the tank temperature at 18-22 ℃± 1 ℃. The wall thickness of the titanium heat exchanger should be sufficient (1.0-1.5mm) to prevent perforation under sulfuric acid and high flow rates.

5.2 Special components for micro arc oxidation

Micro arc oxidation (MAO) generates a hard ceramic film on the surface of aluminum, magnesium, and titanium alloys by applying a higher voltage (400-600V) on the basis of anodic oxidation. The components of its power supply equipment and mixing system have special characteristics.

The output power of the dedicated high-voltage pulse power supply can reach 100-500kW, with a peak current of several thousand amperes. Internal power devices (IGBT) require forced water cooling, output cables must use high-voltage shielded wires, and connection terminals require special insulation treatment. The cathode is made of stainless steel plate, and the distance between the cathode and the anode workpiece needs to be precisely controlled within the range of 50-200mm. Fluctuations in the distance will directly affect the breakdown voltage and film uniformity.

The stirring and cooling system is more important in micro arc oxidation - strong discharge generates a large amount of heat, requiring high flow circulation (10-20 tank volumes per hour) and efficient cooling (titanium plate heat exchanger). At the same time, the suspended ceramic particles in the electrolyte need to be removed through a filtration system (5-10 μ m filter element), but the filtration amount should not be too large to avoid removing nanoparticles that are beneficial for film formation.

6、 Components in thermal spraying process

Thermal spraying uses a heat source (flame, arc, plasma) to heat the sprayed material to a molten or semi molten state, and sprays it at high speed onto the surface of the pre treated workpiece to form a coating, which is used to repair dimensions and provide wear-resistant or corrosion-resistant functional layers.

6.1 Spray gun components

The core components of a plasma spray gun include a cathode (tungsten electrode containing thorium or lanthanum), an anode (copper nozzle), an insulator, and a powder feeding tube. A high-temperature arc is generated between the cathode and anode (temperature can reach over 15000 ℃), and the working gas (argon, helium, hydrogen or nitrogen) is ionized to form a plasma jet. The cathode tip will gradually passivate due to high-temperature erosion, affecting the stability of the arc and the power of the spray gun. Generally, it needs to be replaced or polished every 50-100 hours of operation. The anode nozzle is susceptible to both thermal erosion and powder erosion, and an enlarged aperture can cause plasma jet divergence and a decrease in spraying efficiency, making it one of the vulnerable components.

The High Speed Flame Spray Gun (HVOF) burns oxygen with fuel (kerosene, propane, or propylene) to produce a high-speed flame (with a speed of up to 2000m/s). The key components include the combustion chamber, nozzle, and powder feeding assembly. The combustion chamber can withstand high temperatures (about 3000 ℃) and high pressures (1-2MPa), and must be made of heat-resistant alloys (such as Inconel 625 or 718) and equipped with forced water cooling. The nozzle wears out quickly under high-speed powder containing airflow erosion, and is often protected by tungsten carbide coating, which is still a vulnerable part.

6.2 Powder feeder and cooling system

The powder feeder requires stable and uniform feeding of powder into the spray gun. The structure of the gravity powder feeder is simple, but the powder feeding amount is greatly affected by the flowability of the powder; The groove type powder feeder precisely measures powder through slotted wheels, and the fluctuation of powder feeding can be controlled within ± 2%, which is suitable for the preparation of high-quality coatings. The components inside the powder feeder that come into contact with the powder, such as wheel grooves, scrapers, and pipelines, should be made of wear-resistant materials (ceramic coatings or hard alloys).

Most spray gun cooling systems use deionized water circulation cooling to prevent water scaling and blockage. The cooling water pump needs to provide sufficient flow (usually 5-15L/min), control the outlet temperature below 35 ℃, and the high temperature alarm interlock is a necessary function to prevent the spray gun from burning out.

7、 Tooling components in chemical heat treatment (carburizing, nitriding)

Chemical heat treatment improves performance by changing the surface chemical composition, and the process is carried out in a high-temperature atmosphere furnace. The heat resistance and lifespan of tooling components directly affect production efficiency and cost.

7.1 Carbonization tooling components

The carburizing material tray, material frame, and positioning fixture need to be repeatedly used at high temperatures of 920-950 ℃ to withstand the weight of the workpiece and the corrosion of the carburizing atmosphere (including CO and H ₂). Heat resistant steel (such as Cr25Ni20Si2, Cr28Ni48W5) is a traditional material, but its lifespan is limited, with approximately 200-300 heats in an air furnace. In recent years, high-temperature alloys such as HK40 and HP40, as well as heat-resistant steel fixtures treated with surface aluminum infiltration, have significantly improved their oxidation and carburizing resistance, and their service life can be extended to 500-800 heats.

The fixed carbon sheet is a small consumable component used to detect the carbon potential of furnace gas, and is made of ultra-thin (0.08-0.10mm) pure iron foil. After staying in the furnace for a certain period of time, the carbon plate is taken out and weighed or burned for analysis to determine the carbon content, and the carburizing atmosphere is adjusted accordingly. The accuracy of the carbon plate directly affects the accuracy of the carbon concentration distribution in the carburized layer.

7.2 Nitriding tooling components

The nitriding temperature is relatively low (500-560 ℃), but it requires high resistance to nitriding of the fixture - stainless steel will generate nitrides in the nitriding atmosphere, causing the fixture to become brittle. Pure titanium tooling has become a high-quality tooling material for ion nitriding and gas nitriding due to its dense titanium nitride layer on the surface, which can prevent nitrogen from diffusing into the interior, and its thermal expansion coefficient matches well with the parts. However, the cost is high. The nitriding material tray can also be coated with nickel or aluminum on the surface of low carbon steel, which is both economical and has certain resistance to nitriding.

8、 Surface inspection and quality control components

The final determination of surface treatment quality depends on testing instruments and standard components.

Coating thickness gauge is used to measure the thickness of coatings or coatings. The magnetic thickness gauge is suitable for non-magnetic coatings on steel substrates, and the magnetic core (cobalt iron alloy) and Hall element in its probe are key components; The eddy current method thickness gauge is suitable for non-conductive coatings on non-ferrous metal substrates, and the coil accuracy and temperature stability of the probe affect the measurement accuracy. Standard thickness sheets (plastic or metal foils of known thickness) are used for daily calibration of thickness gauges, and should be traced back to national standards, while avoiding bending and contamination.

The grid cutter is used for coating adhesion testing and consists of a multi blade cutting tool (with tip spacing of 1mm, 2mm, or 3mm) and a guiding device. The tool material is hard alloy, with a cutting edge angle of 15-30 ° and 6 or 11 evenly spaced teeth. The tool must be replaced after wear or missing teeth on the blade, otherwise the cutting will be uneven and the adhesion rating will be distorted.

The roughness comparison block is used to evaluate the surface roughness after sandblasting, shot blasting, or coating. The sample blocks are processed by electroplating or precision milling to produce surfaces with different Ra values (usually Ra 0.1-100 μ m), and the operator compares them with the workpiece surface through touch or vision. The sample block needs to be regularly inspected, and if there are scratches or wear on the surface, it will no longer be used.

The parts in the salt spray test box need to be corrosion resistant: the box is made of PP or PVC plate, the nozzle in the spray tower is made of borosilicate glass or PTFE, and the salt water bucket and collector are made of salt spray resistant materials. If the nozzle aperture (0.5~1.0mm) is blocked or worn, causing the spray volume to deviate from the standard requirements (1~2ml/80cm ² · h), the test results are not credible.

9、 The technological development trend of surface treated components

9.1 Green and environmentally friendly material substitution

Traditional surface treatment extensively uses toxic and harmful substances (hexavalent chromium, cyanide, lead, cadmium, etc.), and their alternative processes have put forward new requirements for components. For example, trivalent chromium plating replaces hexavalent chromium plating, and the anode material is changed from lead based alloy to DSA titanium anode. It is required that the anode can still work stably in a fluoride free and catalyst free sulfate system. Cyanide free galvanizing requires the use of alkaline plating solution, which requires higher alkali resistance for the anode and tank body. The promotion of environmentally friendly surface treatment processes has directly promoted the material upgrade and structural optimization of related components.

9.2 Automation and Intelligent Equipment Components

The application of intelligent equipment such as robot automatic spraying, automatic shot blasting, and automatic loading and unloading has put forward higher requirements for the repeated positioning accuracy, wear resistance life, and integration with sensing systems of surface treated components. For example, the reliability of internal seals (perfluoroether rubber) and valve cores (ceramic or hard alloy) of color changing valves (multi-channel, quick wash type), precision flow control valves, and spray gun cleaning devices for robot spraying directly affects the stability and color changing efficiency of automatic spraying. The flow sensor and wear monitoring system in intelligent shot blasting equipment need to provide real-time feedback on shot blasting volume, blade wear, and other information to the control system to achieve adaptive adjustment of process parameters.

9.3 Synergy between additive manufacturing and surface treated components

Additive manufacturing technology is changing the supply model of surface treated components. For example, by using 3D printing to manufacture sandblasting nozzles with optimized structure (optimized internal flow channel topology), energy loss can be further reduced; Printing a thermal spray gun body with a conformal cooling channel can solve the problem of uneven heat dissipation in traditional drilling cooling channels. The surface treatment industry itself is also utilizing additive manufacturing to repair high-value components (such as ultra poor repair of plasma sprayed coatings on turbine blades), forming a composite technology route of "additive+surface".

9.4 Online Monitoring and Predictive Maintenance

By installing vibration, temperature, pressure, flow and other sensors on key components such as shot blasting machines, spray guns, and filtration systems, combined with IoT technology, online status monitoring and predictive maintenance of surface treatment equipment can be achieved. For example, monitoring the vibration spectrum of the impeller of the shot blasting machine, and automatically alerting when the imbalance caused by blade wear reaches the set threshold; Monitor the pressure difference between the inlet and outlet of the electroplating filter, calculate the remaining life of the filter element, and prompt for replacement. This transition from passive maintenance to active warning reduces unplanned downtime and improves overall equipment utilization.

10、 Conclusion

The application of components in the surface treatment industry covers the entire process from pre-treatment to post-treatment, from equipment body to process accessories, from quality inspection to environmental control. The material selection, structural design, and maintenance of key components such as shot blasting blades, spray gun nozzles, electroplating anodes, carburizing fixtures, and coating thickness probes directly affect the quality of surface treatment products and the economic efficiency of the process.

Different surface treatment processes have their own emphasis on the core requirements of components: shot blasting cleaning emphasizes the ability of components to resist erosion and wear; Painting focuses on nozzle atomization and electrostatic adsorption performance; Electroplating has strict requirements for corrosion resistance and conductivity of anodes, fixtures, and filtration systems; Anodizing requires titanium cathodes and precision cooling systems; The spray gun and powder feeder of thermal spraying determine the upper limit of coating quality; Chemical heat treatment fixtures must maintain sufficient oxidation and creep resistance in a high-temperature atmosphere environment.

Looking ahead to the future, with stricter environmental regulations, rising labor costs, and increasing demands for surface quality in the manufacturing industry, surface treated components are developing towards high performance (long lifespan, resistance to harsh environments), greenness (non-toxic materials, energy-saving design), and intelligence (sensor integration, adaptive adjustment). For surface treatment equipment manufacturers, process engineers, and frontline operators, a deep understanding of the performance characteristics of components, scientific selection and maintenance of components, and active follow-up of technological innovation are important paths to enhance surface treatment competitiveness and achieve high-quality manufacturing. Only by striving for excellence in every detail of each component can we ultimately achieve high-quality surfaces that meet the demanding requirements of modern industry.

Tel
15921227578 Liu Jinlin
Landline:021-69176937
Email
jinlinliu@bmzpmw.com
Headquarters Base
No. 58, Lane 355, Shengxin South Road, Nanxiang Town, Jiading District, Shanghai
Taicang Base
About 60 meters northeast of the intersection of Taicang City Pai Xin Chang Line and Xingang Road in Suzhou City
Customer Service WeChat
Copy successful
Contact
We are right beside you
Add WeChat and let us know your needs
Tel
15921227578
Top
Copy successful